Pure Metal 99.994% Lead Ingots Aluminum Alloy Zinc Ingot Tin Ingot With Cheap Price Manufacturer
1. Primarily utilized in the die-casting alloy battery industry for its superior quality and performance.
2. Extensively applied in the Painting, Printing, Dyeing, Pharmaceutical, and Rubber industries, among others.
3. Essential in chemical industries, particularly in zinc and other metal alloy plating and coating applications.
4. Vital for zinc plating, brass manufacture, manganese bronze, galvanized iron, dry batteries, and as a catalyst and reducing agent.
Brand |
Chemical | |||||||||
Zn(≥) | Impurity(≤) | |||||||||
Pb | Cd | Fe | Cu | Sn | Al | As | Sb | Totsal | ||
Zn99.995 | 99.995 | 0.003 | 0.002 | 0.001 | 0.001 | 0.001 | 0.001 | -- | -- | 0.005 |
Zn99.99 | 99.99 | 0.005 | 0.003 | 0.003 | 0.002 | 0.001 | 0.002 | -- | -- | 0.01 |
Zn99.95 | 99.95 | 0.03 | 0.01 | 0.02 | 0.002 | 0.001 | 0.01 | -- | -- | 0.05 |
Zn99.5 | 99.5 | 0.45 | 0.01 | 0.05 | -- | -- | -- | 0.005 | 0.01 | 0.5 |
Zn98.5 | 98.5 | 1.4 | 0.01 | 0.05 | -- | -- | -- | -- | -- | 1.5 |
ltimate tensile strength | 331 MPa (270 MPa aged) | 48,000 psi (39,000 psi aged) |
Yield strength (0.2% offset) | 295 MPa | 43,000 psi |
Impact strength | 52 J (56 J aged) | 38 ft-lbf (41 ft-lbf aged) |
Elongation at F max | 2% | |
Elongation at fracture | 3.6% (13% aged) | |
Shear strength | 262 MPa | 38,000 psi |
Compressive yield strength | 600 MPa | 87,000 psi |
Fatigue strength (reverse bending 5x10 8 cycles) | 57 MPa | 8,300 psi |
Hardness | 114 Brinell | |
Modulus of elasticity | 96 GPa | 14,000,000 psi |
Solidification range (melting range) | 380386 °C | 716727 °F |
Density | 6.7 kg/dm 3 | 0.24 lb/in 3 |
Coefficient of thermal expansion | 27.4 μm/m-°C | 15.2 μin/in-°F |
Thermal conductivity | 109 W/mK | 756 BTU-in/hr-ft 2 -°F |
Electrical resistivity | 6.54 μΩ-cm at 20 °C | 2.57 μΩ-in at 68 °F |
Latent heat (heat of fusion) | 110 J/g | 4.7x10 -5 BTU/lb |
Specific heat capacity | 419 J/kg-°C | 0.100 BTU/lb-°F |
Coefficient of friction | 0.08 |